для заказа - sumitomo@sumitomo-tools.ru
Wave Mill Series
WEX Type
Recommended Cutting Conditions
WEX2000 Series 12,5mm
Cutter: WEX2025E Insert: AXMT123508PEER - 3mm
Cutting Data: ap = 3mm, ae = 12,5mm, dry Chipbreaker ACP100 ACP200 Coated Carbide ACM200 „Diamond like Carbon“
ISO Material HB Coated Carbide
ACP300 ACK200 ACK300
Feed Rate (mm/tooth) ACM300 DL1000
0,08 0,15 0,20 0,08 0,15 0,20 0,08 0,15 0,20 0,08 0,15 0,20 0,08 0,15 0,20 0,08 0,15 0,20 0,08 0,15 0,20 0,05 0,15 0,22
Unalloyed steel, <0, 15%C, annealed Cutting Speed vc (m/min)
„ , <0, 45%C, annealed 125 G 380 350 330 350 330 315 330 315 295
190 G 285 255 235 255 235 220 235 220 220
„ , <0, 45%C, tempered 250 G 235 210 190 210 190 170 190 170 150
„ , <0, 75%C, annealed 270 G 190 162 143 171 152 133 152 133 115
„ , <0, 75%C, tempered 300 G 145 115 95 115 95 75 95 75 55
180 G 265 235 220 235 220 200 220 200 180
P Low alloyed steel, annealed 275 G 170 145 125 150 130 115 130 115 95
300 G 150 125 105 135 115 95 115 95 75
„ , tempered 350 G 125 95 75 105 85 65 85 65 45
„ , tempered
„ , tempered
High alloyed and tool steel, annealed 200 G 235 210 190 210 190 170 190 170 150
„ , tempered 325 G 125 95 75 95 75 55 75 55 35
Stainless steel, ferritic/martensitic, annealed 200 E 175 155 125 155 140 110
160 140 110 145 125 100
M Martensitic, tempered 240 EH 190 170 140 170 150 125
Austenitic, plunged 180 E
K Grey cast iron G 285 255 235 255 235 220
Nodular cast iron G 190 160 140 160 140 125
S High tempered resist. alloys, Fe based, annealed 300 E 50 40 45 35
„ , hardened 330 E 35 25 30 20
Aluminium alloy, Si < 13% S 1000 750 500
S 250 200 170
N Aluminium alloy, Si > 13% S 350 330 300
Copper alloy
The above recommended cutting conditions are meant as a guide. Actual conditions will depend on the individual machine, work shape and clamping. They will need to be
adjusted according to machine rigidity, work clamp rigidity, cutting depth and other factors.
For groove milling, reduce the feed rate approximately 70% of the corresponding value shown above.
WEX3000 Series 16mm
Cutter: WEX30325E Insert: AXMT170508PEER - 5mm
Indexable
Endmills
Chipbreaker
Cutting Data: ap = 5mm, ae = 16mm, dry Coated Carbide „Diamond like Carbon“
ISO Material Coated Carbide
ACP100 ACP200 ACP300 ACK200 ACK300 ACM200 ACM300 DL1000
HB Feed Rate (mm/tooth)
0,12 0,25 0,35 0,12 0,25 0,35 0,12 0,25 0,35 0,12 0,25 0,35 0,12 0,25 0,35 0,12 0,25 0,35 0,12 0,25 0,35 0,05 0,15 0,25
Cutting Speed vc (m/min)
Unalloyed steel, <0, 15%C, annealed 125 G 400 370 350 370 350 330 350 330 310
„ , <0, 45%C, annealed 190 G 300 270 250 270 250 230 250 230 210
„ , <0, 45%C, tempered 250 G 250 220 200 220 200 180 200 180 160
„ , <0, 75%C, annealed 270 G 200 170 150 180 160 140 160 140 120
„ , <0, 75%C, tempered 300 G 150 120 100 120 100 80 100 80 60
P Low alloyed steel, annealed 180 G 280 250 230 250 230 210 230 210 190
„ , tempered 275 G 180 150 130 160 140 120 140 120 100
„ , tempered 300 G 160 130 110 140 120 100 120 100 80
„ , tempered 350 G 130 100 80 110 90 70 90 70 50
High alloyed and tool steel,annealed 200 G 250 220 200 220 200 180 200 180 160
„ , tempered 325 G 130 100 80 100 80 60 80 60 40
Stainless steel, ferritic/martensitic, annealed 200 E 185 165 135 165 150 120
M Martensitic, tempered 240 EH 170 150 120 150 135 110
180 E 200 180 150 180 160 135
Austenitic, plunged
K Grey cast iron G 300 270 250 270 250 230
Nodular cast iron G 200 170 150 170 150 130
S High tempered resist. alloys, Fe based, annealed 300 E 50 30 45 25
„ , hardened 330 E 50 30 45 25
Aluminium alloy, Si < 13% S 1000 750 500
N Aluminium alloy, Si > 13% S 250 200 170
Copper alloy S 350 330 300
The above recommended cutting conditions are meant as a guide. Actual conditions will depend on the individual machine, work shape and clamping. They will need to be
adjusted according to machine rigidity, work clamp rigidity, cutting depth and other factors.
For groove milling, reduce the feed rate approximately 70% of the corresponding value shown above.
H20 www.sumitomo-tools.ru